Effect of Aluminum Purity on the Pore Formation of Porous Anodic Alumina
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Kim, Byeol | - |
dc.contributor.author | Lee, Jin Seok | - |
dc.date.available | 2021-02-22T12:01:08Z | - |
dc.date.issued | 2014-02-10 | - |
dc.identifier.issn | 0253-2964 | - |
dc.identifier.issn | 1229-5949 | - |
dc.identifier.uri | https://scholarworks.sookmyung.ac.kr/handle/2020.sw.sookmyung/10976 | - |
dc.description.abstract | Anodic alumina oxide (AAO), a self-ordered hexagonal array, has various applications in nanofabrication such as the fabrication of nanotemplates and other nanostructures. In order to obtain highly ordered porous alumina membranes, a two-step anodization or prepatterning of aluminum are mainly conducted with straight electric field. Electric field is the main driving force for pore growth during anodization. However, impurities in aluminum can disturb the direction of the electric field. To confirm this, we anodized two different aluminum foil samples with high purity (99.999%) and relatively low purity (99.8%), and compared the differences in the surface morphologies of the respective aluminum oxide membranes produced in different electric fields. Branched pores observed in porous alumina surface which was anodized in low-purity aluminum and the size; dimensions of the pores were found to be usually smaller than those obtained from high-purity aluminum. Moreover, anodization at high voltage proceeds to a significant level of conversion because of the high speed of the directional electric field. Consequently, anodic alumina membrane of a specific morphology, i.e., meshed pore, was produced. | - |
dc.format.extent | 4 | - |
dc.language | 영어 | - |
dc.language.iso | ENG | - |
dc.publisher | WILEY-V C H VERLAG GMBH | - |
dc.title | Effect of Aluminum Purity on the Pore Formation of Porous Anodic Alumina | - |
dc.type | Article | - |
dc.publisher.location | 독일 | - |
dc.identifier.doi | 10.5012/bkcs.2014.35.2.349 | - |
dc.identifier.scopusid | 2-s2.0-84894525434 | - |
dc.identifier.wosid | 000332265200003 | - |
dc.identifier.bibliographicCitation | BULLETIN OF THE KOREAN CHEMICAL SOCIETY, v.35, no.2, pp 349 - 352 | - |
dc.citation.title | BULLETIN OF THE KOREAN CHEMICAL SOCIETY | - |
dc.citation.volume | 35 | - |
dc.citation.number | 2 | - |
dc.citation.startPage | 349 | - |
dc.citation.endPage | 352 | - |
dc.type.docType | Article | - |
dc.identifier.kciid | ART001850243 | - |
dc.description.isOpenAccess | N | - |
dc.description.journalRegisteredClass | sci | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
dc.description.journalRegisteredClass | kci | - |
dc.relation.journalResearchArea | Chemistry | - |
dc.relation.journalWebOfScienceCategory | Chemistry, Multidisciplinary | - |
dc.subject.keywordPlus | ORDERED ARRAY | - |
dc.subject.keywordPlus | OXIDE | - |
dc.subject.keywordPlus | TEMPERATURE | - |
dc.subject.keywordPlus | LAYER | - |
dc.subject.keywordPlus | FILMS | - |
dc.subject.keywordPlus | FABRICATION | - |
dc.subject.keywordPlus | MEMBRANES | - |
dc.subject.keywordPlus | ACID | - |
dc.subject.keywordPlus | SIZE | - |
dc.subject.keywordAuthor | Porous anodic alumina | - |
dc.subject.keywordAuthor | Impurities | - |
dc.subject.keywordAuthor | Electric field | - |
dc.subject.keywordAuthor | Branched pore | - |
dc.subject.keywordAuthor | Meshed pore | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
Sookmyung Women's University. Cheongpa-ro 47-gil 100 (Cheongpa-dong 2ga), Yongsan-gu, Seoul, 04310, Korea02-710-9127
Copyright©Sookmyung Women's University. All Rights Reserved.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.